Troughput: max. 200kg/h Material: PET granules Bulk density: 830-850kg/m³ Inlet moisture: 2000ppm Outlet moisture: <100ppm With sufficient crystalline material. (experience shows > 15%) In the case of low crystallinity, drying at temperatures > 80°C can lead to clumping (same effect as in the DA). The material can then also be dried at 80°C, but the moisture after the dryer will then be < 600ppm and the dosage should then be reduced to approx. 7% (140kg/h). Max. throughput: 200 kg/h Hopper volume: 1400L - screw on, plug in and start - electric power supply only - no water connection - no installation on-site - lowest energy consumption - nearly service free - WLAN connectivity to your mobile device Voltage: 3x____V/__Hz Description & Documentation: English interfaces: to be defined Installation: to be defined |